Definition

Doping means the introduction of impurities into the semiconductor crystal to deliberately change its conductivity due to deficiency or excess of electrons. In contrast to the doping during the wafer fabrication, where the entire wafer is doped, this article describes the partial doping of silicon. The introduction of foreign substances can be achieved by diffusion, ion implantation (or alloy).

Diffusion

Molecular diffusion, often called simply diffusion, is a net transport of molecules from a region of higher concentration to one of lower concentration by random molecular motion. The result of diffusion is a gradual mixing of materials. To illustrate: a drop of ink in a glass of water is evenly distributed after a certain amount of time. In a silicon crystal, one finds a solid lattice of atoms through which the dopant has to move. This can be done in different ways:

Diffusion

The dopant can diffuse as long as either a concentration gradient is balanced, or the temperature was lowered, so that the atoms can no longer move. The speed of the diffusion process depends on several factors:

Diffusion with an exhaustible source: Diffusion with an exhaustible source means that the dopant is available in a limited amount only. The longer the diffusion process continues, the lower the concentration at the surface, and therefore the depth of penetration into the substrate increases. The diffusion coefficient of a substance indicates how fast it moves in the crystal. Arsenic with a low diffusion coefficient penetrates slower into the substrate, as for example phosphorus or boron.

Diffusion with an inexhaustible source: In diffusion processes with an inexhaustible source the dopants are available in unlimited amount, and therefore the concentration at the surface remains constant during the process. Particles that have penetrated into the substrate are continually replenished.

Diffusion methods

In the subsequent processes the wafers are placed in a quartz tube that is heated to a certain temperature.

Diffusion from the gas phase: A carrier gas (nitrogen, argon, ...) is enriched with the desired dopant (also in gaseous form, e.g. phosphine PH or diborane BH) and led to the silicon wafers, on which the concentration balance can take place.

Diffusion with solid source: Slices which contain the dopants are placed in-between the wafers. If the temperature in the quartz tube is increased, the dopant from the source discs diffuses into the atmosphere. With a carrier gas, the dopant will be distributed uniformly, and thus reaches the surface of the wafers.

Diffusion with liquid source: As liquid sources boron bromide BBr or phosphoryl chloride POCl can be used. A carrier gas is led through the liquids and thus transporting the dopant in gaseous state. Since not the entire wafers should be doped, certain areas can be masked with silicon dioxide. The dopants can not penetrate through the oxide, and therefore no doping takes place at these locations. To avoid tensions or even fractions of the discs, the quartz tube is gradually heated (e.g. +10 °C per minute) till 900 °C. Subsequent the dopant is led to the wafers. To set the diffusion process in motion, the temperature is then increased up to 1200 °C.

Characteristic:
Doping mask

Ion implantation

In the ion implantation charged dopants (ions) are accelerated in an electric field and irradiated onto the wafer. The penetration depth can be set very precisely by reducing or increasing the voltage needed to accelerate the ions. Since the process takes place at room temperature, previously added dopants can not diffuse out. Regions that should not be doped, can be covered with a masking photoresist layer.

An implanter consists of the following components:

Illustration of an ion implanter

Ion implanter

Penetration depth of ions in the wafer: In contrast to diffusion processes the particles do not penetrate into the crystal due to their own movement, but because of their high velocity. Inside the crystal they are slowed down by collisions with silicon atoms. The impact causes damage to the lattice since silicon atoms are knocked from their sites, the dopants themselves are mostly placed interstitial. There, they are not electrically active, because there are no bonds with other atoms which may give rise to free charge carriers. The displaced silicon atoms must be re-installed into the crystal lattice, and the electrically inactive dopants must be activated.

Recovery the crystal lattice and activation of dopants: Right after the implantation process, only about 5 % of the dopants are bond in the lattice. In a high temperature process at about 1000 °C, the dopants move on lattice sites. The lattice damage caused by the collisions have already been cured at about 500 °C. Since the dopants move inside the crystal during high temperature processes, these steps are carried out only for a very short time.

Channeling: The substrate is present as a single crystal, and thus the silicon atoms are regularly arranged and form "channels". The dopant atoms injected via ion implantation can move parallel to these channels and are slowed only slightly, and therefore penetrate very deeply into the substrate. To prevent this, there are several possibilities:

Channeling

Characteristic:

There are several types of implanters for small to medium doses of ions (1011 to 1015 ions/cm2) or for even higher doses of 1015 to 1017 ions/cm2.

The ion implantation has replaced the diffusion mostly due to its advantages.

Doping using Alloy For completeness it should be mentioned that besides ion implanation and diffusion there is an alternative process: doping using alloy. Since this procedure, however, brings disadvantages with it such as cracks in the substrate, it is not used in today's semiconductor technology any more.